Skip Navigation



The European Journal of Orthodontics Advance Access published online on June 9, 2009

The European Journal of Orthodontics, doi:10.1093/ejo/cjp035
This Article
Right arrow Full Text
Right arrow Full Text (PDF)
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Email this article to a friend
Right arrow Similar articles in this journal
Right arrow Similar articles in PubMed
Right arrow Alert me to new issues of the journal
Right arrow Add to My Personal Archive
Right arrow Download to citation manager
Right arrowRequest Permissions
Google Scholar
Right arrow Articles by Uysal, T.
Right arrow Articles by Kurt, G.
PubMed
Right arrow PubMed Citation
Right arrow Articles by Uysal, T.
Right arrow Articles by Kurt, G.
Social Bookmarking
 Add to CiteULike   Add to Connotea   Add to Del.icio.us  
What's this?

© The Author 2009. Published by Oxford University Press on behalf of the European Orthodontic Society. All rights reserved. For permissions, please email: journals.permissions@oxfordjournals.org.

Evaluation of shear bond strength of metallic and ceramic brackets bonded to enamel prepared with self-etching primer

Tancan Uysal, Ayca Ustdal and Gokmen Kurt

Department of Orthodontics, Faculty of Dentistry, Erciyes University, Kayseri, Turkey

Address for correspondence Dr Tancan Uysal, Erciyes Universitesi, Dis Hekimligi Fakultesi, Ortodonti AD, Melikgazi, Kayseri 38039, Turkey, E-mail: tancanuysal{at}yahoo.com


   Abstract

The aim of this in vitro study was to evaluate the shear bond strength (SBS) of different metallic and ceramic bracket bonding combinations using self-etching primers (SEPs). Eighty freshly extracted human premolar teeth were randomly divided into four equal groups for bonding with ceramic or metallic brackets as follows: group 1, metallic brackets bonded with conventional acid etching; group 2, metallic brackets bonded with Transbond Plus Self-Etching primer (TPSEP); group 3, ceramic brackets bonded as per group 1; group 4, ceramic brackets bonded as per group 2. The SBS of these brackets was measured and recorded in megapascals (MPa). The adhesive remnant index (ARI) scores were determined after bracket failure. Data were analyzed with the analysis of variance, Tukey, and chi-square tests.

The bond strength of group 3 (mean: 36.7 ± 11.8 MPa) was significantly higher than group 4 (mean: 26.6 ± 8.9 MPa; P < 0.05), group 1 (mean: 25.5 ± 5.1 MPa; P < 0.01), and group 2 (mean: 22.9 ± 7.3 MPa; P < 0.001). No significant differences in debond locations were found among the groups (P > 0.05). Compared with conventional acid etching, SEPs significantly decreased the SBS of ceramic orthodontic brackets.


Add to CiteULike CiteULike   Add to Connotea Connotea   Add to Del.icio.us Del.icio.us    What's this?




Disclaimer: Please note that abstracts for content published before 1996 were created through digital scanning and may therefore not exactly replicate the text of the original print issues. All efforts have been made to ensure accuracy, but the Publisher will not be held responsible for any remaining inaccuracies. If you require any further clarification, please contact our Customer Services Department.